Neirynck & Vogt N.V. - Lebanon

Neirynck & Vogt N.V. - Lebanon 25 years’ experience of innovation for high technology investment materials.

We guarantee high precision castings and continuous high quality results for all dental applications.

Time to bring Z 4 - C&B Universal Investment to your lab? Let me know1- CASTING2- CAD / CAST3- PRESSING4- 3D PRINT🌐 www....
12/05/2025

Time to bring Z 4 - C&B Universal Investment to your lab? Let me know

1- CASTING
2- CAD / CAST
3- PRESSING
4- 3D PRINT

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
*Hachem Line* – NV distributor in Lebanon

N&V TipsHelpful tips for pressable ceramics Pressable ceramics have become a top choice of many clinicians because of th...
28/04/2025

N&V Tips
Helpful tips for pressable ceramics

Pressable ceramics have become a top choice of many clinicians because of their ability to create such esthetically pleasing restorations. With Universal Z4 Investment and Disposable Plungers being great choices for improving pressing results, we've had an opportunity to help many dental laboratories troubleshoot different types of problems.

Many of the newer all-ceramic materials can be tricky to use at first and users must often make adjustments to "dial in" their results. With that in mind we thought we would share a few of the problems and solutions we commonly see… Soon

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

Time to bring Z4 Universal Investment to your lab?Metal C&B Work casting done by one of our talented Lebanese Dental Tec...
25/03/2025

Time to bring Z4 Universal Investment to your lab?
Metal C&B Work casting done by one of our talented Lebanese Dental Technicians using Z4 Universal Investment!

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

N&V TipsHelpful tips for casting alloysQuestion: After sandblasting, I have a couple of edgy rough spots on the castingA...
19/03/2025

N&V Tips
Helpful tips for casting alloys

Question: After sandblasting, I have a couple of edgy rough spots on the casting

Answer: In this case it is perhaps not bad to have a look at your wax pattern under microscope before investing. Sometimes one is surprised to see how many dust particles are on the surface of the pattern. It may be gypsum dust, grains of sand blasting material or any other scrap sticking to the wax. By using Z4, a very fine flowing investment that reproduces every detail, the scrap will be perfectly cast and visible on the surface of the casting. Cleaning the wax before investing with dry air or water may be the solution here. Better still is to work in a clean environment for waxing up. Ideal is to not wax up on the same spot as where you finish the metal!

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

Time to bring MG-Vest Investment to your lab?Partial Denture casting done by one of our talented Lebanese Dental Technic...
15/03/2025

Time to bring MG-Vest Investment to your lab?
Partial Denture casting done by one of our talented Lebanese Dental Technicians using MG-Vest!

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

N&V TipsHelpful tips for casting alloysQuestion: The casting comes a bit rough out of the investment and I have a hard t...
13/03/2025

N&V Tips
Helpful tips for casting alloys

Question: The casting comes a bit rough out of the investment and I have a hard time sand blasting the metal

Answer: This is an indication of overheated metal. The metal may not be burned but it is overheated. The best way to check if the metal was cast at the right time is to just pass your finger over the button or cone of the casting. If the edge feels sharp, the metal was heated too much. The edge should be rounded as a clear indication of the right casting temperature. As a result of casting at the right temperature the castings will come clean of investment with just some oxidizing on the metal depending on the kind of metal used.

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

🌐 www.hachemline.comπŸ“§ dental@hachemline.com☎️ (01)684061 πŸ“±+961 3 924 158Hachem Line – NV distributor in Lebanon
09/03/2025

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

Z4… Faster.. Much Faster

Z4… "Rapid Cast" Universal Investment can be placed into the preheating furnace after 30 minutes, 3 hours, 3 days, or 3 weeks later at any given temperature without the fear of inconsistent results or exploding cylinders!

🌐 www.hachemline.com
πŸ“§ dental@hachemline.com
☎️ (01)684061 πŸ“±+961 3 924 158
Hachem Line – NV distributor in Lebanon

19/02/2025
16/02/2025

Address

120 JMJ Center 5-24 Etihad StreetSt-Elie ResidencesNew Rawda, Maten
Beirut

Opening Hours

Monday 09:00 - 17:00
Tuesday 09:00 - 17:00
Wednesday 09:00 - 17:00
Thursday 09:00 - 17:00
Friday 09:00 - 17:00
Saturday 09:00 - 13:00

Telephone

+9613924158

Alerts

Be the first to know and let us send you an email when Neirynck & Vogt N.V. - Lebanon posts news and promotions. Your email address will not be used for any other purpose, and you can unsubscribe at any time.

Contact The Practice

Send a message to Neirynck & Vogt N.V. - Lebanon:

Share

Z4 Universal Investment

Imagine an investment that allows you to cast the finest rpd frames, crowns, facings inlays or onlays in whatever alloy or ceramic ingot you require!

Z4 Universal Investment. Your partner for every technique!